HDPE

High-density polyethylene wax (HDPE) is polymerized to deliver high stability, low oil absorption, and high hardness, making it suitable for most thermoplastic formulations.
GradeDropping Point(°C)Viscosity(cPs)Physical Form
LP0020P113≤20Powder
LP1020P11610–20Powder
LP0100F11340–100Flake
LP8110F112≤40Flake

LDPE

OX102P comes from low-density polyethylene (LDPE) via oxidation treatment, offering polar groups, strong wetting capability, and high suitability for pigment dispersion and coating materials.
GradeDropping Point(°C)Viscosity(cPs)Physical Form
OX102P104200Powder

Thermally Cracked PE Wax

WD2040PX is produced via thermal cracking technology, offering low viscosity, strong wetting ability, and excellent thermal stability, making it particularly suitable for color masterbatches and high-shear processing.
GradeSoftening Point(°C)Viscosity(cPs)Physical Form
WD2040PX109320–480Powder