Introduction
IPPP and CDP are liquid phosphate esters that function both as flame retardants and plasticizers.
| Product | Appearance | Phosphorus Content (%) | Color (APHA) | Specific Gravity (20°C) | Acid Value (mg KOH/g) | Water Content (%) |
|---|---|---|---|---|---|---|
| IPPP | Colorless to Pale Yellow Transparent Liquid | ≧8.3 | ≦50 | 1.16–1.18 | ≦0.1% | ≦0.1% |
| CDP | Colorless to Pale Yellow Transparent Liquid | ≧9.1% | ≦50 | 1.197–1.215 | ≦0.1% | ≦0.1% |
This product contains IPPP/CDP components, which are classified as Substances of Very High Concern (SVHC) under the EU REACH regulation. If the concentration in the formulation exceeds 0.1 wt%, information disclosure and safety assessment are required in accordance with regulatory requirements.