The test sample successfully passed the UL 94 V-0 flame retardancy standard. After two separate flame applications, the sample self-extinguished within 10 seconds each time, with no flaming drips igniting the cotton below. This indicates that the material possesses the highest level of vertical flame retardancy, demonstrating outstanding safety and reliability.

The test sample successfully passed the UL 94 V-0 flame retardancy standard. After two separate flame applications, the sample self-extinguished within 10 seconds each time, with no flaming drips igniting the cotton below. This indicates that the material possesses the highest level of vertical flame retardancy, demonstrating outstanding safety and reliability.