Introduction
JUYEE high-quality mica powder, including phlogopite and muscovite, suitable for a wide range of applications such as engineering plastics, coatings, and construction materials. With its layered structure, high aspect ratio, and excellent heat resistance, mica is an ideal choice as a functional filler
Application Advantages of Mica
MicaFort mica powder features high purity and stability, making it suitable for a wide range of applications including engineering plastics, coatings, and construction materials.
- In engineering plastics, it effectively enhances material rigidity and dimensional stability.
- In coatings, it reinforces film structure and improves corrosion resistance and weatherability.
- In construction materials, mica powder enhances structural stability and heat resistance. It also offers excellent fire resistance and thermal insulation, making it suitable for diverse applications such as composite panels, insulation layers, and high-performance coatings.
Phlogopite
Phlogopite is a hard, plate-like powder composed of an iron-, magnesium-, and potassium-containing aluminum silicate. Due to its high aspect ratio, it provides excellent stiffness and dimensional stability in plastic applications, while also enhancing heat resistance. It is commonly used in automotive components and marine anti-corrosion coatings.
| Grade | Surface Treatment | Particle Size D50 | Aspect Ratio |
|---|---|---|---|
| PW30 | None | 18 μm | 86 |
| PW30S | Treated | 18 μm | 86 |
| PW80 | None | 35 μm | 110 |
| PW80S | Treated | 35 μm | 110 |
Origin: Finland
Related Links
Muscovite
White powder that does not affect color formulation.
| Grade | Surface Treatment | Particle Size D50 | Aspect Ratio |
|---|---|---|---|
| SX300 | None | 14 μm | 38 |
Origin: United Kingdom