Vinyl Resin Application Guide

Vinyl resins are widely used in inks, coatings, adhesives, and surface treatment systems. Due to differences in molecular structure and functional modification, each grade offers unique advantages in adhesion, chemical resistance, film formation, and processing performance.

The following guide summarizes the common applications and recommended substrates for Sinfeng and Hanwha vinyl resins as a reference for product selection.

Ink Applications

Application Recommended Grades
Application Recommended Grades
Gravure Inks MVAG, PG-HC
Screen Printing Inks MVAG, MVOH, VMA
PVC Inks MLC-14-55, MLC-10-80
Paper Inks LC-40
Reflective Inks MVAG
UV Inks TLC-40/43, PG-HC
Vinyl resins provide excellent adhesion, pigment wetting, and printing performance, making them suitable for a wide range of ink formulations.

Coating Applications

Application Recommended Grades
Wood Coatings MVAG, MVOH
Toy Coatings MLC-14-55, MLC-10-80
Plastic Coatings MVAG, PG-HC
Automotive Refinish Coatings MVAG
UV Coatings TLC-40/43, PG-HC
UV Varnishes TLC-40/43, PG-HC
Can Coatings VMA
The proper selection of vinyl resin can improve adhesion, durability, chemical resistance, and overall coating performance.

Adhesive and Surface Treatment Applications

Application Recommended Grades
PVC Adhesives LC-40, MLC-10-80
Leather Treatment Adhesives MLC-14-55, MLC-10-80
Hot Stamping Foil Primers VAMA, VMA
Coil Nail Adhesives VAMA
EVA Primers VMA
PU Color Chips LC-40, MLC-14-55
PU White Ink Systems LC-40, MLC-14-55
Peelable Coatings MLC-10-80
Adhesive and surface treatment systems generally require strong adhesion and compatibility with various substrates. Proper grade selection is therefore critical.

Recommended Grades by Substrate

Substrate Recommended Grades
PET MVAG, MVOH, PG-HC
PVC MVAG, MVOH, PG-HC, TLC-40/43, VAMA, VMA
ABS MVAG, MVOH, VAMA, VMA
PC VMA, TLC-40/43
PA MVAG, VAMA, VMA
Aluminum Foil VAMA, VMA
Tinplate VAMA, VMA

Hanwha binary vinyl copolymers are widely used in adhesives, inks, coatings, and overprint varnish systems.

ApplicationCP-430CP-450CP-710
Adhesives★★★
Printing Inks★★★
Industrial Coatings★★★
Overprint Varnishes★★★
Flooring Coatings ★ 
 

Conclusion

The selection of vinyl resin depends on application requirements, substrate type, and processing conditions. Different grades provide varying levels of adhesion, chemical resistance, film-forming properties, and durability. By choosing the appropriate resin grade, formulators can optimize the performance of inks, coatings, adhesives, and surface treatment systems.

For more information about specific grades and technical data, please visit JUYEE’s Vinyl Resin product pages or contact our technical team.