Overview

PVC (Polyvinyl Chloride) is a polymer produced by the polymerization of vinyl chloride monomers and is one of the five major general‑purpose resins.
With mature processing technology, PVC is widely used in building materials and consumer products.
Depending on customer requirements, it can be processed through impregnation, coating, rotational molding, molding, spraying, and other methods.

JUYEE offers two categories of PVC emulsion powders: general‑grade emulsion powders and functional PVC powders.

General‑Grade Emulsion Powders

Product CodePhysical PropertiesApplication Description
PF621K Value: 62.9
*Brookfield Viscosity: 78
*Severs Viscosity: 65
Suitable for applications requiring high whiteness and high‑expansion
foaming
• Wallpaper
• Printing inks
PG680 (68GP)K Value: 69.2
*Brookfield Viscosity: 33
*Severs Viscosity: 81
Provides uniform foaming quality and fine foam structure,
with smooth foam surfaces and higher whiteness
• Synthetic leather (foam layer)
• Wallpaper
• Flooring (foam layer / backing layer)
• Filament and mesh coating
• Automotive sealants
PG740 (74GP)K Value: 74.4
*Brookfield Viscosity: 30
*Severs Viscosity: 89
• Canvas
• Synthetic leather (surface layer)
• Automotive sealants
• Conveyor belts
• Flooring (surface layer)
• Wire and mesh coating
• Toys, tool grips, terminal sleeves
• Printing inks
PC750 (75HC)K Value: 76.1
*Brookfield Viscosity: 31
*Severs Viscosity: 91
Suitable for products requiring high transparency and glossy appearance
• High‑gloss tarpaulin
• Glossy synthetic leather surface
• Flooring / logo mats
• Cosmetic and mesh coatings
• Toys, logos, transparent terminal sleeves
PG770 (77GP)K Value: 79.3
*Brookfield Viscosity: 28
*Severs Viscosity: 99
• Disposable gloves
• Synthetic leather (high‑strength surface layer)
• High‑weather‑resistant tarpaulin
• Wire harness and mesh coating
• PVC tiles and commercial flooring surface
• Metal can inner coatings (food‑contact grade)
• Automotive sealants

*Brookfield Viscosity (ASTM D1824) → Low shear, used to evaluate resting/slow processing flow behavior, affecting foaming and coating.
*Severs Viscosity (RY-W-QC-E030) → High shear, used to evaluate high-speed processing rheology, affecting spraying and extrusion stability.

PVC Toys
Wallpaper
Waterproof Fabric
Disposable Gloves

Related Links

Functional PVC Powders

Product CodePhysical PropertiesApplication Description
KR‑51Fine‑matte specialty PVC powder
Appearance: White powder
K‑Value: ~70
Excellent matte effect.
Used in synthetic leather, impregnation, wallpaper, canvas,
toys, etc.
K13SCoarse‑matte specialty PVC powder
Appearance: White powder
K‑Value: 69.8–72.8
For PVC impregnation or soft/hard PVC extrusion where a more pronounced matte texture is required.
KCM‑12Low‑temperature‑gelation PVC powder
Composition: VC/VAc copolymer
VAc: 5.5 ± 2%
K‑Value: 63.3–67.6
Low‑temperature gelation with good adhesion.
Suitable for fabrics, carpets, synthetic leather, metal or automotive primers, and sealants.
KR‑16PVC viscosity‑reducing powder
Composition: PVC 100%
K‑Value: 66
Density (g/cm³): 0.59 ± 0.05
Degree of Polymerization (30 °C): 1000 ± 50
Used to reduce the viscosity of PVC plastisols.
Its excellent viscosity‑reducing effect improves flowability, especially in formulations with lower plasticizer content.
PBM‑B5FEconomic‑grade PVC viscosity‑reducing powder
Appearance: White powder
K‑Value: 66.1–69.0
Bulk Density: 0.45–0.65
Provides viscosity reduction and matting. Mainly used in flooring, wallpaper, toys, synthetic leather, treadmill belts, hand tools, and more.
Base Grade (Glossy Black Finish)
Fine Mist KR-51
Recommended Addition Level: 45%–50%
Coarse Mist K13S
Recommended Addition Level: 40%–50%
Wallpaper
Synthetic Leather
Fitness Equipment Handle