Introduction

In high-filler formulations, dispersants play a crucial role. They not only influence the dispersion uniformity of pigments and fillers, but also directly dictate processing performance, surface quality, and production efficiency. Below are our empirical test results for dispersants across various material systems, providing objective data and visual comparisons to assist you in selecting the optimal formulation.

PVC Formulation Testing: Impact of Dispersants on TiO2 Dispersion Quality

  • Objective : Compare the dispersion effects of different dispersants on TiO2 within PVC matrix systems.

  • Key Highlights :

    • Q-300: A dispersant that provides rapid wetting and highly effective dispersion for inorganic materials, delivering outstanding performance.

    • LDP-110: A hyperdispersant that exhibits exceptional dispersion performance for inorganic fillers and inorganic pigments.

TPE Formulation Comparison: Performance Differences in TiO2 Dispersion

  • Objective : Investigate the performance differences between Q-300 and LDP-110 in dispersing TiO2 within TPE matrix systems.

  • Key Highlights :

    • Q-300: A dispersant that rapidly wets and effectively disperses inorganic materials, delivering outstanding performance.

    • LDP-110: A hyperdispersant that demonstrates exceptional dispersion results for inorganic fillers and inorganic pigments.

Inorganic Filler Testing: Dispersion Effect Analysis of CaCO3 & ATH

  • Objective : Test the dispersion capability of Q-300 and LDP-110 on calcium carbonate CaCO3 and aluminum hydroxide (ATH).

  • Key Highlights :

    • Q-300 provides rapid wetting of inorganic powders with stable dispersion performance.

    • LDP-110 maintains superior flowability and dispersibility even under high-filler loadings.

Weathered UPVC Formulation Testing: Impact of Dispersants on Whiteness & Fineness

  • Objective : Test the dispersion effectiveness of dispersants on TiO2 and blue pigments within weathered UPVC formulations.

  • Key Highlights :

    • Q-350 achieved full color development and demonstrated the best fineness performance.

    • Dispersants significantly improve specimen appearance and color uniformity.

Technical Summary & Application Guidelines

  • Dispersant selection must be tailored according to filler type, concentration, and processing conditions.

  • High-efficiency dispersants effectively reduce viscosity, enhance flowability, and improve surface finish quality.