Introduction
CPP (Chlorinated Polypropylene) is a thermoplastic resin modified by chlorination. It is commonly used in inks, primers, and coating formulations. This product belongs to the chlorinated polypropylene resin family and is primarily designed to enhance adhesion.
Characteristics
Excellent adhesion to polypropylene (PP).
Good adhesion to polyethylene (PE), paper, and aluminum film.
Acts as an adhesion‑promoting resin for inks, primers, coatings, and adhesives.
Good solubility; chlorine content and viscosity can be selected to suit different formulations.
Applications
Inks
Composite inks
Chlorinated inks (toluene‑based and ester‑based types)
Improves adhesion in polyurethane inks
Primers
Promotes adhesion to substrates such as PP, PE, and aluminum films
Coatings
Used for plastic surface coatings
Functions as an adhesion‑promoting resin
Adhesives
- Enhances bonding with low‑surface‑energy materials such as PP and PE
Product Specifications
| Model | Appearance | Viscosity (mPa·s) | Chlorine Content (%) | Recommended Solvents | Recommended Applications |
|---|---|---|---|---|---|
| S200 | Light yellow granules | 120–220 | 30 | Toluene / Methylcyclohexane | Benzene‑soluble chlorinated inks |
| S300 | Light yellow granules | 250–350 | 30 | Toluene | Ink |
| L200-25 | Light yellow granules | 150–250 | 25 | Toluene | Coating |
| H250-36 | Light yellow granules | 150–250 | 36 | n-Propyl Acetate / Ethyl Acetate | Ester‑soluble chlorinated inks |
| H10-38 | Light yellow granules | 5–10 | 40 | Ethyl acetate | Polyurethane Ink |
| MS300 | Light yellow granules | 250–350 | 30 | n‑Propyl acetate | Coatings, adhesives |