Introduction

The JUYEE powdered calcium‑zinc stabilizer series is specifically designed for PVC products, offering excellent heat stability, processability, and insulation properties. It is suitable for a wide range of applications including wires and cables, pipes, flooring, and edge bands. Compliant with environmental and safety standards, various models are available to meet different processing requirements.

Transparent Products

ModelApplication AreaFeatures and Uses
HT6881G High‑transparency productsHigh transparency; maintains color stability over time.
HT6881R High‑transparency soft productsTransparency comparable to organic tin stabilizers; fast plasticization rate; maintains color stability during long‑term processing.

Wires, Cables & Plugs

ModelApplication AreaFeatures and Uses
CZ-2021White UL105°CExcellent insulation performance with good heat resistance, color stability, and gelation properties.
CZ-36-105 Black and Colored UL105°C Electronic WiresMeets UL105°C aging requirements; good flowability, fine appearance, excellent heat resistance, and non‑exudation.
CZ-38-105White UL105°C electronic wireMeets UL105°C aging requirements; good initial color and high color retention after aging.
HT6801BWhite electronic wire, plugSuitable for standard white wires; stable whiteness, non‑yellowing over time, economical formulation.
HT6802B2Black and Colored Electronic Wires, Flexible Tubes, and PlugsSuitable for standard black wires; good processability, economical formulation, ideal for low aging performance requirements.
HT6802F2Sheath, cableAging requirement 70–90°C; Congo red ≥100 minutes.
HT6809J2Sheath, cableAging requirement ≥90°C; Congo red ≥180 minutes.
HT6809QUL125°C automotive wire, charging gunAging requirement 125°C; Congo red ≥240 minutes.

Pipes & Fittings

ModelApplication AreaFeatures and Uses
HT6811Water supply and drainage pipesSuitable for products with diameters of 20–630 mm; compatible with calcium carbonate ≤ 20 phr. Excellent heat stability, high whiteness, and stable physical properties. Widely applicable to water supply and drainage pipes. For scratch‑resistant requirements, high‑heat ACR is recommended.
HT6811F7Drainage pipesSuitable for non‑standard drainage pipes; compatible with calcium carbonate 50–200 phr.
HT6811F8-1 Drainage pipesSuitable for international‑standard drainage pipes; compatible with calcium carbonate 15–100 phr. High whiteness, strong versatility, and cost‑effective performance.
HT6821B6Drainage fittingsCompatible with calcium carbonate 20–50 phr; economical formulation.
HT6821E9-5Water supply fittingsSuitable for products with diameters ≤ 75 mm; compatible with calcium carbonate ≤ 8 phr. Excellent flowability and whiteness; can replace organotin stabilizers.
HT6821E11DWater supply fittingsSuitable for products with diameters of 20–400 mm; compatible with calcium carbonate 3–8 phr. High whiteness and good flowability; can replace organotin stabilizers.

Profiles & Extruded Materials

ModelApplication AreaFeatures and Uses
HT6831D3Profiles, sealing strips, honeycomb panelsSuitable for extruded profiles; offers high cost‑performance ratio.
HT6831GDoor and window framesCompatible with calcium carbonate 25–75 phr; free of color pigments.
HT6831G4Door and window framesExcellent plasticization performance; suitable for twin‑screw extrusion and compatible with 16–30 phr calcium carbonate.
HT6831G4-1Door and window framesDesigned for European‑standard door and window profiles; contains ultramarine for stable color tone and high cost‑performance ratio.

PVC Flooring

ModelApplication AreaFeatures and Uses
HT6812F1SPC FlooringSPC composite flooring product with excellent thermal stability and slip resistance. Promotes plasticization and enhances surface gloss. Offers outstanding oxidation and aging resistance, superior weatherability, and extended continuous production cycles.
HT6812LLVT FlooringDesigned for LVT flooring applications; provides good processability and a smooth surface finish.

Calendered Film, Sheet Material & Synthetic Leather

ModelApplication AreaFeatures and Uses
HT6851GWhite or colored rigid calendered sheetSuitable for non‑transparent products.
HT6851YGeneral synthetic leather surface layerCan replace powder or liquid calcium‑zinc and barium‑zinc stabilizers.
HT6851QAutomotive synthetic leather surface layerCan replace Galata stabilizers.

CPVC Series

Model Application AreaFeatures and Uses
HT830APipe materials and fittingsCan replace 30% of organotin stabilizer in equal quantity; effectively improves Vicat softening temperature.
HT6871CPipe materials and fittingsCan completely replace organotin stabilizer. Recommended addition ratio: 1.2–1.5 : 1. Provides excellent plasticization performance and superior thermal stability compared to organotin stabilizers.