Liquid Stabilizer Catalog

Product CategoryModelApplicationsApplications & Features
Transparent ProductsCN-37Flexible or
Semi-Rigid PVC
High-Concentration Liquid Barium-Zinc Stabilizer
High concentration, excellent heat resistance,
and good initial color for transparent applications.
Transparent ProductsLTX-630Flexible PVCHigh-Concentration Liquid Calcium-Zinc Stabilizer
Excellent stability and transparency.
Foam ProductsNKFoamed ProductsHas excellent foaming control and stability.