PVC PASTE RESIN

                 *:25 ℃±0.5 ℃,DOP 60phr

 GradeK Value*Brookfield viscosityApplication
 62GP(PG620)623200Foam layer for synthetic leather, wallpaper,
PVC flooring, adhesives and other low fusion products.
 68GP(PG680)683400Foam layer for synthetic leather, wallpaper, Tarpaulin, auto sealants, adhesives, screen coating.
 74GP(PG740)742900Top skin layer for synthetic leather, Tarpaulin, screen coating, trademark, toy, yoga ball,
metal dipping, PVC floor surface, sealing strip of car, electronic terminal sets.
 77GP(PG770)772700Surface layer of synthetic leather, gloves,
PVC floor surface, screen printing.
 75HC(PC750)753200Coating, trademark and other transparent demand products.

PVC MATTING AGENT

KR-51 Special PVC Resin, fine matting effect, mat surface, good touching feeling, reduce viscosity.