Brief and application

Phlogopite is a hard flake powder and an aluminosilicate containing iron, magnesium and potassium.
Due to it has high diameter-to-thickness ratio,
It has good stiffness and dimensional stability in plastic applications, and can also improve the heat resistance of plastics.
Used in auto parts, and also in anti-corrosion coatings for ships.

GradeSurface treatmentParticle size d50Aspect ratio
 PW30None18 μm86
 PW30SYes18 μm86
 PW80None35 μm110
 PW80SYes35 μm110