PVC PASTE RESIN

  • General grades (GP): 62GP、68GP、 74GP、 77GP (number is K value)
  • Transparent grade: 75HC Matting agent: KR-51
  • Vinyl Resin (Chloroethylene – Vinyl Acetate Copolymer, Chloroethylene – Vinyl Acetate Copolymer- Maleic Acid Terpolymers)

Mexichem CR80 Copolymer series – Application on strippable coating、PVC ink

  • Sinfeng Carboxyl-Modified Vinyl Chloride/Vinyl Acetate terpolymers: Application on the adhesive for strip nail、coil nails, marine paint, ink for metal, lacquer for aluminum foil
  • Sinfeng Hydroxyl-Modified Vinyl Chloride/Vinyl Acetate terpolymess: Application on anti-corrosion coatings, gravure inks, chassis paints, PET inks
  • Sinfeng Hydroxyl-Modified Vinyl Chloride/Vinyl Acetate terpolymers: MVAH、MTA5R、PG-HC (Ester soluble)

Flame Retardant

  • Inorganic flame retardant UltraCarb: Good char forming, application on PVC、LSOH、EPDM、aluminum plastic composite panel
  • Isopropylated triphenyl phosphate(Liquid): It is a kind of plasticizer and also the liquid flame retardant, compliance with Environmental regulations, application on PVC、PU、Epoxy.
  • Antimony trioxide:General Grade 99.5 %、 High purity 99.8 %

PVC stabilizer

  • CZ-2017 Ca-Zn powder
  • BN-612 Ba-Zn powder
  • MCZ-235 Mg-Ca-Zn powder (transparent, nontoxic, odorless)
  • CN-40 Ba-Zn liquid
  • WR-01 Ca-Zn powder (fulfillment of W specification for UL outdoor wire)
  • LTX-630 Ca-Zn liquid

Function Plasticizer

  • B-70: quick gelatinization with low temperature, good compatibility, application on PVC, NBR, PU and TPU
  • W-1300: a kind of plasticizer for reducing viscosity

Dispersant

  • Q300 liquid dispersant: It is able to disperse TiO2, calcium carbonate and inorganic.
  • LDP-110: Super dispersant

滑劑

  • RG-60: Internal ester lubricant
  • RG-19: Internal and external ester lubricant
  • RG-70: Internal and external ester lubricant
  • PE WAX (WD 2040P): External lubricant

Functional filler- Mica

  • Widely used in various industrial plastic products such as PP, PA, Nylon, PBT…It can enhance the rigidity, stability and buckling resistance of plastic products.

Thickening

  • FS-200 is the hydrophilic fumed silica, with thixotropy, reinforcing and thickening effects

UV Absorber

  • UV-1/UV-2/UV-960 UV absorber (liquid): Application on TPU, PU (soft and hard foam, elastic fiber)

Non-PVC plastisol

  • AP103
  • AP303

TPE (THERMOPLASTIC ELASTOMER)

  • Application on wire cables, connectors and various customization wire cables.